Slight bubbling effect on the interior of the solid first layer. It causes no problems.
The bed temperature is 50C, PLA. The wipe and the shells adhere well, the second layer is smooth, the bed is level.
Uneven first layer.. bed temperature?
- LePaul
- Reactions:
- Posts: 3996
- Joined: February 7th, 2016, 10:26 pm
- Location: Bangor, Maine USA
- 3D Printer(s): 24 - Yes I have a problem!
- Contact:
Re: Uneven first layer.. bed temperature?
Photo? Printer type? Material?